abstract = "The aim of this study was to develop new soft contact lens (SCL) materials which would,
after recommended and existing machining processes, improve surface roughness.
Nanomaterials (fullerene, fullerol and methformin hydroxylate fullerene) were
incorporated into commercial material for SCL (SL38) based on PHEMA, which were
derived by the technology in the production lab of the company Soleko (Milan, Italy).
Nanophotonic SCLs (SL38-A, SL38-B, SL38-C, respectively) were produced in the company
Optix (Belgrade, Serbia) from the obtained materials. For the surface characterization of
SCLs, AFM analysis and lacunarity method were performed. The results showed that for
the SL38-B average roughness value is lower than those of SL38-A and SL38. The
topography parameters of SL38-C were between the parameters of SL38-A and SL38-B.
Lacunarity analysis of AFM images confirmed that SCLs surface state should belong to
either group of adequate (slanted p-diagram) or inadequate (contorted p-diagram)
roughness concerning tear film stability. Nanophotonic SCL SL38-C exibits more acceptable
performance considering SCL surface functional behavior as compared to other SCLs. The
positive result of incorporating nanomaterials into basic material for SCL is better quality
of the nanophotonic SCLs surfaces. On the bases of these experiments, the assumption
that incorporation of fullerene derivate will not increase surface roughness parameters is
confirmed., U ovom radu predstavljeni su novi materijali za meka kontaktna sočiva
(MKS), koja bi nakon preporučene mašinske obrade imala poboljšana
svojstva hrapavosti površine. Nanomaterijali (fuleren, fulerol i metformin
hidroksilata fulerena) su inkorporirani u bazni materijal za MKS (SL38), u
čijoj je osnovi poli(2-hidroksietil metakrilat), pо tеhnоlоgiјi i u
prоizvоdnim lаbоrаtоriјаmа kоmpаniје Soleko (Milano, Italija). Od
dobijenih materijala napravljena su nanofotonična MKS (SL38-A, SL38-B i
SL38-C, redom) u kompaniji Optix (Beograd, Srbija). Površinska
karakterizacija izvršena je Miskorskopijom atomskih sila (MAS) i metodom
lagunarnosti. Rezultati su pokazali da SL38-B ima niže vrednosti osnovnog
parametra hrapavosti od SL38-A i SL38. Za SL38-C, vrednosti parametara
topografije bili su između vrednosti parametara nanofotoničnih mekih
kontaktnih sočiva SL38-A i SL38-B.
Analiza lagunarnosti MKS potvrđuje stanje površine sočiva ili kao
adekvatno (nagnut p-dijagram) ili kao neadekvatno (iskrivljen p-dijagram),
a s obzirom na naknadnu stabilnost suznog filma. Nanofotonično MKS u
oznaci SL38-C ispoljava prihvatljivije performanse po pitanju
funkcionalnog ponašanja u poređenju sa ostalim MKS.
Dobijeni su pozitivni rezultati inkorporiranja nanomaterijala u bazni
material, koji pokazuju bolji kvalitet površina nanofotoničnih MKS. Na
osnovu ovih eksperimenata potvrđeno je da inkorporiranje derivata
fulerena ne utiče na porast parametara hrapavosti površine.",
publisher = "Association of the Chemical Engineers of Serbia",
journal = "HEMIJSKA INDUSTRIJA",
title = "Characterization of surface roughness of new nanophotonic soft contact lenses using lacunarity and AFM method, Karakterizacija hrapavosti površine novih nanofotoničnih mekih kontaktnih sočiva mikroskopijom atomskih sila i metodom lagunarnosti",
pages = "166-157",
number = "3",
volume = "72",
doi = "10.2298/HEMIND170924004M"
}